Why the lead lag dryer midpoint matters
At a polyethylene plant, the obvious place to check feed moisture is the reactor outlet. That reading has a problem though: if it shows water, the water has already reached the reactor. By then, the catalyst may be losing activity, co-catalyst is being consumed and the resin coming out may be drifting off grade.
A measurement point one step further upstream gives you something the reactor inlet cannot: time to act.
Why does the reactor inlet measurement come too late? Moisture at the reactor inlet is a variable final check but it is not an early warning measurement. If the reading rises there, water has already passed through the feed treating system and entered the reactor. In a polyethylene process, even trace moisture can affect catalyst performance, consume co-catalyst and contribute to changes in polymer properties. The objective is therefore not simply to detect water at the reactor, it is to detect it before it reaches the reactor.
Polymer grade ethylene normally passes through feed treaters before it reaches the reactor. These beds remove oxygen, carbon monoxide, water and other catalyst poisons.
Water is commonly removed by 3A molecular sieve dryers, often installed as a lead lag pair. The lead bed carries most of the drying duty. The lag bed provides a safety margin, catching moisture that breaks through the lead bed before it can reach the reactor.
A molecular sieve bed holds water until its adsorption front approaches the outlet. From that point, water can begin to pass through the bed. The problem is that normal process measurements may not show this happening. Without continuous moisture measurement, the lead bed can break through with little warning, while the lag bed starts consuming its own capacity.
Why the midpoint gives the earliest warning
A dewpoint transmitter between the lead and lag beds sees breakthrough as soon as it begins. At that moment the lag bed is still protecting the reactor.
A rising reading at the midpoint is therefore a warning, not an upset. Operators have time to switch beds, take the lead bed offline and begin regeneration before water reaches the reactor. The reactor does not see the water, so catalyst activity, reaction rate and resin grade are protected. What could have become a reactor upset becomes a planned bed change.
That is why the lead lag midpoint is the primary continuous measurement point in an ethylene feed train.
How to measure moisture at the midpoint
Use a continuous, intrinsically safe dewpoint transmitter. Ethylene is a gas group IIB hazard and analyser locations are commonly classified Zone 1 or Zone 2. An intrinsically safe transmitter can send a 4–20 mA signal to the DCS, where it can be trended, alarmed and used to prompt a bed switch.
The measurement should be based on a representative, conditioned sample of the ethylene vapour. The sample system should be designed to avoid condensation, adsorption and delay.
Watch the trend, not only the value
Polymer grade ethylene is commonly controlled at low ppm(v) moisture levels, with many plants using an alarm or control target below 1 ppm(v). Molecular sieve dryers can condition the gas well below this level.
At atmospheric pressure, 1 ppm(v) of water corresponds to a frost point of about −76 °C. Near that level, the ±2 °C dewpoint accuracy of an aluminium oxide sensor spans roughly 0.75 to 1.4 ppm(v). That does not make the measurement unreliable. It means alarm limits should be set with the measurement band in mind. A steady upward trend at the midpoint is often more meaningful than a single reading because it can indicate the early stages of dryer breakthrough.
Record sample pressure
Pressure changes the dewpoint for a given water content. At 30 bar, the same 1 ppm(v) reads near −52 °C. Always log the sample pressure alongside the dewpoint. If the pressure is not recorded, it can be difficult to distinguish a genuine change in moisture content from a change in sample pressure.
Heat and control the pressure reduction
Ethylene cools as it expands. Its critical temperature is only 9.2 °C, so an unheated regulator on a high pressure line can chill the sample and cause partial condensation. Keep sample lines short and made from stainless-steel. Sample in the vapour phase, apply controlled heat where required and route the vent to flare or another safe location.
Allow the sample system to stabilise
Below 1 ppm(v), water held on tubing walls and fittings and other wetted surfaces can continue to desorb for some time after a line has been opened or disturbed. Purge a new or disturbed sample line with process gas and wait for a flat trend before relying on the reading. A stable baseline is essential when measuring trace moisture.
Use midpoint data to optimise dryer cycles
Many plants switch dryer beds on a fixed timer. That approach is safe but it can be conservative: beds may be regenerated before they have used their full available capacity. A midpoint moisture trend shows how much capacity each cycle actually uses and how much is left unused. With that data, regeneration intervals can be optimised rather than guessed. The result can be fewer unnecessary regenerations, reduced energy consumption and better use of dryer capacity, without compromising reactor protection.
Build a complete ethylene moisture strategy
The lead lag midpoint is the key measurement but it works best as part of a wider moisture monitoring plan:
Battery limit
Measure moisture at the battery limit to check incoming ethylene against the supply specification before it loads the treaters.
Reactor feed header
Measure moisture at the reactor feed header for final assurance that nothing downstream of the lag bed is adding water.
After regeneration or maintenance
Use an intrinsically safe portable hygrometer to spot check a bed after regeneration or maintenance, confirming that it is dry before it returns to service.
Learn more about dewpoint measurement in ethylene feed gas
Our application note, Dewpoint Measurement in Ethylene Feed Gas, covers all four measurement points, the relevant standards and our recommended instruments.
Shaw Moisture Meters has designed and built dewpoint instruments for over seventy years. Tell us about your requirements and we’ll help you choose the right instrument for your ethylene feed gas application. Contact us.